RussPitcher wrote:I engrave anodized aluminium dog tags regularly. This works very well in a single pass using a tungsten carbide replacement tip. When I had a diamond tip I found that a single pass produced a fine line that didn't quite remove all the anodizing and two passes created a thicker line that left clean aluminium so with the right SVG I could get two styles of line.
Pressure: 200
Speed: 240mm/s
Up Speed: 500mm/s
I just set tool depth using the spacer as usual.
Shout if you need any help.